Civil EngineeringVery hard
IS 10262 mix design for 20 mm nominal size aggregate: base water content 186 kg/m³ for 50 mm slump, increased by 3% for each further 25 mm slump. For a slump of 125 mm and w/c = 0.4, the cement content is
- A. 537.3 kg/m³
- B. 465.0 kg/m³
- C. 506.9 kg/m³
- D. 476.4 kg/m³
Correct answer: C. 506.9 kg/m³
Water = 202.7 kg/m³; cement = water/(w/c) = 202.7/0.4 = 506.9 kg/m³.
Practise more RCC, Steel Structures & Construction Materials (Civil) questionsRCC, Steel Structures & Construction Materials (Civil): notes and key points
More RCC, Steel Structures & Construction Materials (Civil) questions
- IS 10262 mix design for 20 mm nominal size aggregate: base water content 186 kg/m³ for 50 mm slump, increased by 3% for each further 25 mm…
- Absolute-volume method per m³ of concrete: water 186 kg, w/c = 0.45, entrapped air 2%, specific gravities cement 3.15, coarse aggregate…
- Absolute-volume method per m³ of concrete: water 190 kg, w/c = 0.5, entrapped air 2%, specific gravities cement 3.15, coarse aggregate…
- A mix needs 180 kg of free water per m³ with SSD aggregates: CA 1100 kg and FA 700 kg. The field coarse aggregate carries 0% free…
- A post-tensioned tendon of length 30 m (Es = 2×10⁵ N/mm²) draws in 3 mm at the anchorage. The average loss of prestress stress due to…
- A post-tensioned cable is stressed to 1100 kN at the jacking end. Using Px = P0·e^−(μα+kx) with μ = 0.25, total angular change α = 0.1…