Mechanical EngineeringVery hard

A 0.4% carbon steel is slowly cooled from the austenite region (eutectoid 0.76% C, ferrite solubility 0.02% C). The fraction of proeutectoid ferrite is approximately

  1. A. 0.40
  2. B. 0.53
  3. C. 0.72
  4. D. 0.49

Correct answer: D. 0.49

Lever rule: (0.76 - 0.4)/(0.76 - 0.02) = 0.36/0.74 = 0.49.

More Machine Design, Strength of Materials & Vibrations (ISRO Mech) questions

Exams that ask this topic