Restorative Dentistry and ProsthodonticsHard
Which phase of set low-copper amalgam is the weakest and most prone to corrosion?
- A. Gamma-2 (Sn7-8Hg)
- B. Gamma (Ag3Sn)
- C. Gamma-1 (Ag2Hg3)
- D. Eta (Cu6Sn5)
Correct answer: A. Gamma-2 (Sn7-8Hg)
The tin-mercury gamma-2 phase is the weakest and most corrosion-prone phase of conventional amalgam.
Practise more Conservative Dentistry & Endodontics (MDS) questionsConservative Dentistry & Endodontics (MDS): notes and key points
More Conservative Dentistry & Endodontics (MDS) questions
- The hybrid layer formed in dentin bonding consists of:
- The C-factor (configuration factor) and polymerisation shrinkage stress are greatest in which restoration?
- The main antibacterial mechanism of calcium hydroxide as an intracanal medicament is:
- The irrigant best suited to remove the inorganic component of the smear layer is:
- Mixing sodium hypochlorite and chlorhexidine in the canal results in:
- Vertucci type III canal configuration is described as: