Dental Anatomy, Oral Pathology and MaterialsHard
The weakest and most corrosion-prone phase of conventional low-copper amalgam is:
- A. Gamma (Ag3Sn)
- B. Gamma-2 (Sn7-8Hg)
- C. Gamma-1 (Ag2Hg3)
- D. Eta (Cu6Sn5)
Correct answer: B. Gamma-2 (Sn7-8Hg)
The tin-mercury gamma-2 phase corrodes readily, creating porosity and reducing strength.