Dental Anatomy, Oral Pathology and MaterialsVery hard
The softening (solution) heat treatment of a gold casting alloy involves:
- A. Slow cooling from 500 degrees C
- B. Heating to 450 degrees C and air cooling
- C. Heating to about 700 degrees C for 10 minutes followed by quenching
- D. Annealing at the melting point
Correct answer: C. Heating to about 700 degrees C for 10 minutes followed by quenching
Quenching from about 700 degrees C retains the disordered solid solution, which is ductile and soft.
More Dental Materials (MDS) questions
- Which element added to nickel-chromium alloys to improve castability is a recognised health hazard during grinding?
- The main constituent forming the glassy matrix of dental porcelain is:
- Leucite is incorporated in feldspathic porcelains for metal ceramics mainly to:
- Which all-ceramic material cannot be effectively etched with hydrofluoric acid?
- The antibacterial action and dentin bridge stimulation of calcium hydroxide is related to its pH of about:
- Eugenol-containing liners should not be placed beneath composite restorations because eugenol: