Physics (JEE/NEET)Very hardJEE Advanced

The intrinsic carrier concentration of silicon varies as n_i ∝ T^{3/2} e^{−E_g/2kT}. With E_g = 1.1 eV and k = 8.617 × 10⁻⁵ eV/K, the ratio n_i(330 K)/n_i(300 K) is about

  1. A. 8.0
  2. B. 1.9
  3. C. 6.9
  4. D. 1.15

Correct answer: A. 8.0

The exponential factor is exp[(E_g/2k)(1/300 − 1/330)] = exp(1.934) = 6.92. The power-law factor is (1.1)^{1.5} = 1.154. Product ≈ 8.0.

More Semiconductor Electronics questions

Exams that ask this topic